← Back to the chapter · Next detail →

Technical detail · Battery-Life Target Contracts

Charge, energy, and self-discharge

The mAh label measures charge, not energy. Multiplying 225 mAh by a fixed 3.0 V gives 0.675 Wh; multiplying it by the 2.0 V floor gives 0.450 Wh. These are fixed-voltage comparisons, rather than an integration of energy over the discharge curve. For a 225 mAh CR2032 example, assuming 1% annual self-discharge, ten years retain about 90.4% and lose about 21.5 mAh. Renata CR2032 datasheet That hidden loss averages 0.246 microamps, consuming about 9.5% of the chapter’s 2.6-microamp ten-year allowance before the circuit draws current.

← Back to the chapter · Next detail →